Comparison of Cyclic Fatigue Resistance of Two Different Rotary NiTi Instruments (An In-Vitro Study)

1Citations
Citations of this article
7Readers
Mendeley users who have this article in their library.

Abstract

Aim: The aim of this study was to compare the dynamic CFR of M3-ProGold instruments and Pepsi Gold instruments. Material and methods: Eighty files of size 25/.06 of M3 Pro Gold files and Pepsi Gold files (each n = 40) were evaluated for dynamic cyclic fatigue resistance inside two artificial stainless-steel canals with 2 different radii [(60̊curvature, 3 and 5 mm curvature radii) at body temperature and immersed in distilled water at 37° ± 1°C. The NCF (number of cycles to failure) was documented. The data was analysed by the use of ANOVA and Tukey post hoc tests (P ≤ 0.05). Results: The Pepsi Gold instruments had a significantly greater NCF than the M3 Pro Gold files in both canal radii at body temperature. Conclusion: Pepsi Gold instruments have higher CFR than M3 Pro Gold instruments.

Cite

CITATION STYLE

APA

Abd Allah, D. A. E., Nagy, M. M., & Yehia, T. (2024). Comparison of Cyclic Fatigue Resistance of Two Different Rotary NiTi Instruments (An In-Vitro Study). Ain Shams Dental Journal (Egypt), 33(1), 121–126. https://doi.org/10.21608/asdj.2023.216874.1180

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free