Abstract
Resonant soft x-ray absorption measurements at the O K edge on a SrMnO 3/LaMnO3 superlattice show a shoulder at the energy of doped holes, which corresponds to the main peak of resonant scattering from the modulation in the doped hole density. Scattering line shape at the Mn L 3,2 edges has a strong variation below the ferromagnetic transition temperature. This variation has a period equal to half the superlattice superperiod and follows the development of the ferromagnetic moment, pointing to a ferromagnetic phase developing at the interfaces. It occurs at the resonant energies for Mn3+ and Mn4+ valences. A model for these observations is presented, which includes a double-exchange two-site orbital and the variation with temperature of the hopping frequency tij between the two sites. © 2012 American Physical Society.
Cite
CITATION STYLE
Smadici, S., Nelson-Cheeseman, B. B., Bhattacharya, A., & Abbamonte, P. (2012). Interface ferromagnetism in a SrMnO3/LaMnO3 superlattice. Physical Review B - Condensed Matter and Materials Physics, 86(17). https://doi.org/10.1103/PhysRevB.86.174427
Register to see more suggestions
Mendeley helps you to discover research relevant for your work.