Microtensile Bond Strength Between Self-Adhesive Resin Cements and Resin Based Ceramic CAD/CAM Block

3Citations
Citations of this article
17Readers
Mendeley users who have this article in their library.

Abstract

Purpose: The objective of this study is to evaluate and compare the microtensile bond strength (μTBS) of four different self-adhesive resin cements to a resin-based ceramic CAD/CAM block, at the baseline, and after subjecting them to 5,000 thermo-cycles.Materials and Methods: Four self-adhesive dual-cured resin cements; G-CEM LinkAce (GC EUROPE, Leuven, Belgium), RelyX U200 (3M ESPE, Seefeld, Germany), Maxcem Elite (Kerr, CA, USA), TheraCem (Bisco, Schaumburg, USA) were applied to Cerasmart CAD/CAM blocks (GC EUROPE, Leuven, Belgium). CAD/CAM blocks were sectioned into sticks and subjected to μTBS tests at 24 hours, and the other half were subjected to tests after 5000 thermo-cycles. The data were tested by one-way variance analysis (p<0.05). Results: The highest bond strength values were observed in TheraCem, followed by G-CEM LinkAce and RelyX U200, respectively (p<0.05). At the baseline, G-CEM LinkAce, RelyX U200, and Maxcem Elite showed statistically similar results. After 5,000 thermal-cycles, a significant decrease was observed in the bond strength values of G-CEM LinkAce (p<0.05). Conclusion: Between the adhesive cements used in the study, TheraCem showed the highest micro-tensile bond strength values both in the baseline (24h) results, and after the 5,000 thermal-cycle aging procedures.

Cite

CITATION STYLE

APA

Berkman, M., Tuncer, S., Tekçe, N., Karabay, F., & Demirci, M. (2021). Microtensile Bond Strength Between Self-Adhesive Resin Cements and Resin Based Ceramic CAD/CAM Block. Odovtos - International Journal of Dental Sciences, 23(1), 116–125. https://doi.org/10.15517/IJDS.2021.43670

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free