Influence of deformation and molybdenum content on acicular ferrite formation in medium carbon steels

14Citations
Citations of this article
26Readers
Mendeley users who have this article in their library.

Abstract

The present work deals with the influence of deformation and molybdenum content on the subsequent austenite-to-acicular ferrite transformation during continuous cooling in medium carbon microalloyed steels. The results obtained demonstrate that higher deformation temperature induces a finer austenite grain size as a result of austenite recrystallisation processes during cooling down to austenite decomposition temperature. The higher the molybdenum content and severity of deformation are, the finer austenite grain is. Likewise, it was concluded that molybdenum suppress pearlitic microstructure, and clearly delay proeutectoid ferrite field to longer times. By contrast, acicular ferrite transformation is enhanced in molybdenum rich steel, which not only affect the volume fraction but also the morphology of acicular ferrite. © 2006 ISIJ.

Cite

CITATION STYLE

APA

Capdevila, C., Ferrer, J. P., García-Mateo, C., Caballero, F. G., López, V., & De Andres, C. G. (2006). Influence of deformation and molybdenum content on acicular ferrite formation in medium carbon steels. ISIJ International, 46(7), 1093–1100. https://doi.org/10.2355/isijinternational.46.1093

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free