Abstract

This work shows that the powder aerosol deposition (PAD) method allows the formation of films in powder quantities of less than 60 mg, rather than the large amounts that are typically required for conventional powder aerosol deposition systems. This was achieved by changing the operation mode to a discontinuous one, resulting in operation times of several seconds. Semiconducting strontium titanate ferrate SrTi0.65Fe0.35O3−δ (STF35) was used as the powder to prove the equal behavior in terms of adhesion, film quality and electric conductivity compared to conventional powder-aerosol-deposited films.

Cite

CITATION STYLE

APA

Linz, M., Exner, J., Kita, J., Bühner, F., Seipenbusch, M., & Moos, R. (2021). Discontinuous powder aerosol deposition: An approach to prepare films using smallest powder quantities. Coatings, 11(7). https://doi.org/10.3390/coatings11070844

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free