Abstract
Hiba (Thujopsis dolabrata) wood was treated with supercritical carbon dioxide (scCO2) at stepwise temperature increments from 50° to 400°C continuously so that extractives (dichloromethane-soluble and -insoluble phases) and solid residues were obtained. The yield of extractives from hiba wood increased with increasing extraction temperature. The volatile compounds in the dichloromethane-soluble phase from scCO2 extraction at 50°C contained only terpenoids. However, the volatile compounds in the dichloromethane-soluble phase from scCO2 extraction at 300°C not only contained terpenoids but also phenols, furans, hydrocarbons, and organic acids. The yield of β-thujaplicin, which is a useful compound in hiba wood, increased with increasing extraction temperature from 50°C to 300°C; the optimal conditions for extracting β-thujaplicin were 300°C and 19. 61 MPa. Further study of degradated compounds from the cellulosic and lignic materials of hiba wood after stepwise high-temperature scCO2 treatment above 300°C may provide clues to its efficient use. © 2011 The Japan Wood Research Society.
Author supplied keywords
Cite
CITATION STYLE
Ohira, T., Edashige, Y., Matsui, N., & Yatagai, M. (2011). Extraction and decomposition of hiba wood into valuable chemicals using stepwise temperature supercritical carbon dioxide treatment. Journal of Wood Science, 57(3), 226–233. https://doi.org/10.1007/s10086-010-1156-8
Register to see more suggestions
Mendeley helps you to discover research relevant for your work.