The aim of this study is to optimize the composition of geopolymer foam that leads to the highest water absorption. This study utilized Response Surface Methodology (RSM) to analyze the relationship between factors Seawater/Potassium Silicate (SW/KSil), Potassium Hydroxide/Potassium Chloride (KOH/KCl), Sodium Lauryl Ether Sulfate/Benzalkonium Chloride (SLES/BAC) and Hydrogen Peroxide/Nanocellulose (H2O2/NC) and its response, water absorption. The concentration of the alkaline solution is maintained at a low level of Molar Ratio (MR) 2.01-2.53 and 0.320 M to 1.620 M. It was found that all factors are significant with ρ-value < 0.05 except for KOH/KCl. The highest water absorption by geopolymer measured is 35%, in the middle range of all factors. Simple water immersion of 30 days shows no significant physical changes on the geopolymer, proving its rigidity under water.

Cite

CITATION STYLE

APA

Hua, T. C., Norkhairunnisa, M., Wayayok, A., Basri, M. S. M., & Abdullah, M. M. A. B. (2024). Optimisation in Water Absorption of Low Molarity Seawater and Zeolite Based Geopolymer Foam Reinforced with Nanocellulose. Archives of Metallurgy and Materials, 69(2), 553–562. https://doi.org/10.24425/amm.2024.149783

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free