Experimental research on the behaviour of metal active gas tailor welded blanks during single point incremental forming process

5Citations
Citations of this article
24Readers
Mendeley users who have this article in their library.

Abstract

The present paper aims to study the behaviour of Metal Active Gas (MAG) tailor welded blanks during the single point incremental forming process (SPIF) from an experimental point of view. The single point incremental forming process was chosen for manufacturing truncated cone and truncated pyramid shaped parts. The same material (S355) and the same thickness (0.9 mm) were selected for the joining of blank sheets because the main goal of the paper was to study the influence of the MAG welding process throughout the SPIF process. A Kuka robot, equipped with a force transducer and an optical measurement system were used for manufacturing and evaluating the parts by SPIF. The selected output data were major and minor strain, thickness reduction, forces and springback at the SPIF process. Another line test was performed to evaluate the formability in SPIF. The main conclusion of the paper is that during the SPIF process, fractures occur in one side welded blanks even at moderate wall angles, while in the case of double side welded blanks there is a decrease of formability but parts can still be produced at moderate angles (55 degrees) without any problems.

Cite

CITATION STYLE

APA

Oleksik, V., Dobrota, D., Racz, S. G., Rusu, G. P., Popp, M. O., & Avrigean, E. (2021). Experimental research on the behaviour of metal active gas tailor welded blanks during single point incremental forming process. Metals, 11(2), 1–29. https://doi.org/10.3390/met11020198

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free