Abstract
The purpose of the study was to evaluate the effect of MTAD in comparison with EDTA as a final rinse on the shear bond strength of Kerr, Apexit and AH plus. Dentine surfaces of 135 extracted human non-carious maxillary premolars were divided into three groups (n=45). Groups I and II were conditioned with 1.3% NaOCl for 20min, followed by a final rinse of 17% EDTA for 1min and MTAD for 5min respectively. Group III was treated with distilled water. Each group was further divided into three subgroups (n=15). Subgroup 1: Kerr, Subgroup 2: Apexit and Subgroup 3: AH plus. Three-millimetre-long sections of polyethylene tubes were filled with freshly mixed sealer and placed on the dentine surfaces. The bonding between the sealer and dentine surface was evaluated using shear bond testing. The values were statistically evaluated using one way anova followed by Tukey's test. Significant difference was found among the bond strength of the sealers and irrigating regimes. AH plus showed superior bond strength among the tested sealers, when EDTA was employed as the final rinse (P<0.05). MTAD as a final rinse affected the bond strength of AH plus and Apexit, which were significantly lower than the control group. © 2010 The Authors. Australian Endodontic Journal © 2010 Australian Society of Endodontology.
Author supplied keywords
Cite
CITATION STYLE
Gopikrishna, V., Venkateshbabu, N., Krithikadatta, J., & Kandaswamy, D. (2011). Evaluation of the effect of MTAD in comparison with EDTA when employed as the final rinse on the shear bond strength of three endodontic sealers to dentine. Australian Endodontic Journal, 37(1), 12–17. https://doi.org/10.1111/j.1747-4477.2010.00261.x
Register to see more suggestions
Mendeley helps you to discover research relevant for your work.