Wetting of grain boundaries in Al by the solid Al3Mg2 phase

99Citations
Citations of this article
47Readers
Mendeley users who have this article in their library.

This article is free to access.

Abstract

The microstructure of binary Al100-x -Mg x (x = 10, 15, 18 and 25 wt%) alloys after long anneals (600-4000 h) was studied between 210 and 440 °C. The transition from incomplete to complete wetting of Al/Al grain boundaries (GBs) by the second solid phase Al3Mg2 has been observed. The portion of completely wetted GBs increases with increasing temperature beginning from T wsmin = 220 °C. Above T wsmax = 410 °C all Al/Al GBs are completely wetted by the Al 3Mg2 phase.

Cite

CITATION STYLE

APA

Straumal, B. B., Baretzky, B., Kogtenkova, O. A., Straumal, A. B., & Sidorenko, A. S. (2010). Wetting of grain boundaries in Al by the solid Al3Mg2 phase. Journal of Materials Science, 45(8), 2057–2061. https://doi.org/10.1007/s10853-009-4014-6

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free