Multi-modal analysis of oxidation on Fe-Cr-Ni austenitic stainless steel 304 exposed to beyond-design basis temperatures

11Citations
Citations of this article
7Readers
Mendeley users who have this article in their library.
Get full text

Abstract

Stainless Steel 304 is being investigated for accident tolerant claddings. In this investigation, we use multi-modal characterization to evaluate oxidation under laboratory air versus 100% steam at 1200 ºC for 2 h. Air oxidation features Fe(NiMn)O4, Fe3O4, Fe(3−x)CrxO4, and Cr2O3. Steam oxidation produces a dual layer, containing Fe2O3-enriched porous outer layer and sub-surface matrix of Fe3O4/Fe(3−x)CrxO4 with SiO2/Fe(3−x)SixO4. From these findings, we postulate the oxidation mechanism. Arrangement of oxidation products in air corroborates with anticipated diffusion behavior, except Cr2O3. However, arrangement in steam deviates due to presumably intergranular interactions with H2O, resulting in the sub-surface matrix.

Cite

CITATION STYLE

APA

Copeland-Johnson, T. M., Nyamekye, C. K. A., Ecker, L., Bowler, N., Smith, E. A., Rebak, R. B., & Gill, S. K. (2023). Multi-modal analysis of oxidation on Fe-Cr-Ni austenitic stainless steel 304 exposed to beyond-design basis temperatures. Corrosion Science, 218. https://doi.org/10.1016/j.corsci.2023.111167

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free