Correlation between fracture surface morphology and toughness In Zr-based bulk metallic glasses

58Citations
Citations of this article
57Readers
Mendeley users who have this article in their library.
Get full text

Abstract

Fracture surfaces of Zr-based bulk metallic glasses of various compositions tested in the as-cast and annealed conditions were analyzed using scanning electron microscopy. The tougher samples have shown highly jagged patterns at the beginning stage of crack propagation, and the length and roughness of this jagged pattern correlate well with the measured fracture toughness values. These jagged patterns, the main source of energy dissipation in the sample, are attributed to the formation of shear bands inside the sample. This observation provides strong evidence of significant "plastic zone"screening at the crack tip. © 2010 Materials Research Society.

Cite

CITATION STYLE

APA

Suh, J. Y., Conner, R. D., Kim, C. P., Demetriou, M. D., & Johnson, W. L. (2010). Correlation between fracture surface morphology and toughness In Zr-based bulk metallic glasses. Journal of Materials Research, 25(5), 982–990. https://doi.org/10.1557/jmr.2010.0112

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free