Abstract
Loss on ignition (LOI) is a very common method for estimating the volatile species in solid sample. Normally, the measurement of LOI can be convenient and accurate, but for municipal solid waste incineration (MSWI) ash, the process may become intricate due to the complexity of the sample. In the incineration ash, there exist various phases, such as mineral, metal, organic and glass. The reaction and transformation of some materials during heating will influence the measurement. 5 incineration ash samples were selected and tested in this study. LOI content was basically measured at high (850°C) and relatively low (440°C) temperatures. The comparison between these two measurements showed a large difference. X-ray diffraction (XRD) and thermal analysis (TG-DTA) were carried out to investigate the mineral changes and weight losses with different ignition temperatures. The mineralogical analysis suggests that the decomposition of hydrate and carbonate phases cannot be neglected for LOI measurement of incineration. A long-time heating under relatively lower temperature (400∼450°C) compared with soil sample measurement (≥500°C) was recommended by this study.
Cite
CITATION STYLE
Yang, S. (2017). Influence of heating on the weight loss and mineral phase in MSWI ash: LOI of incineration ash. In IOP Conference Series: Earth and Environmental Science (Vol. 61). Institute of Physics Publishing. https://doi.org/10.1088/1755-1315/61/1/012079
Register to see more suggestions
Mendeley helps you to discover research relevant for your work.