Low temperature decomposition of polystyrene

21Citations
Citations of this article
31Readers
Mendeley users who have this article in their library.

Abstract

Styrene oligomers (SOs), of styrene (styrene monomer, SM), 1,3-diphenylpropane (styrene dimer, SD1), 2,4-diphenyl-1-butene (styrene dimer, SD2) and 2,4,6-triphenyl-1-hexene (styrene trimer, ST), had been detected in the natural environments far from industrial area. To confirm SOs formation through thermal decomposition of polystyrene (PS) wastes in the nature, purified polystyrene (SO-free PS) has been shown to decompose at 30 to 150 °C. The SO ratio of SM:SD:ST was about 1:1:5 with ST as the main product. Mass spectrometry with selected ion monitoring was used for the quantitative analysis of the trace amounts of SOs. The rate of PS decomposition was obtained as k (year-1) = 5.177 exp(-5029/T(K)) based on the amount of ST. Decomposition kinetics indicated that not only does drifting lump PS break up into micro/nano pieces in the ocean, but that it also subsequently undergoes degradation into basic structure units SO. According to the simulation at 30 °C, the amounts of SOs in the ocean will be over 400 MT in 2050.

Cite

CITATION STYLE

APA

Kimukai, H., Kodera, Y., Koizumi, K., Okada, M., Yamada, K., Hiaki, T., & Saido, K. (2020). Low temperature decomposition of polystyrene. Applied Sciences (Switzerland), 10(15). https://doi.org/10.3390/app10155100

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free