Silicon dioxide nanotubes prepared by anodic alumina as templates

70Citations
Citations of this article
22Readers
Mendeley users who have this article in their library.
Get full text

Abstract

Aligned slicon dioxide nanotubes with diameters of 30-40 nm synthesized by the sol-gel template method are presented. This process involves the growth of nanotubes from ordered nanochannel-array pores in anodic alumina. For a silica sol aged at room temperature and dipped for 1 rain, nanowires were formed in a shorter period of aging time (2 days); nanotubes connecting with solid nanofibers were obtained in a longer aging time (30 days). The formation of nanotubes depends strongly on the temperature of the sol. For a short dipping time (<1 min), bamboolike nanofibers were prepared when the sol was at high temperature (50 °C); however, perfect nanotubes with the sharp wall were synthetized for the lower sol temperature (5 °C). The lower sol temperature is, the smoother the inside wall of nanotubes is. It is proved that viscosity plays an important role on the morphology of nanotubes.

Cite

CITATION STYLE

APA

Zhang, M., Bando, Y., & Wada, K. (2000). Silicon dioxide nanotubes prepared by anodic alumina as templates. Journal of Materials Research, 15(2), 387–392. https://doi.org/10.1557/JMR.2000.0061

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free