Silver - Based infiltrated composites

11Citations
Citations of this article
13Readers
Mendeley users who have this article in their library.

Abstract

Attempts have been made to describe the influence of production process parameters on the microstructure and properties of W - Ag and Mo - Ag composites. W-30%Ag, W-40%Ag, Mo-30% Ag and Mo-40%Ag composites were produced by tumbling W5%Ag and Mo-5%Ag mixtures for 30 minutes in the Turbula T2F mixer. The powders were subsequently cold pressed inarigid die onasingle action press. The pressure was adjusted individually to assure 25% and 35% green porosity. Prior to infiltration the compacts were sintered in hydrogen at 1100°C for one hour. The porous skeletons were finally contact infiltrated with Ag-1%Ni alloy at 1100 and 1200°C for one hour in hydrogen. The main objective of this work was to compare properties and microstructure of the as-infiltrated composites.

Cite

CITATION STYLE

APA

Madej, M. (2012). Silver - Based infiltrated composites. Archives of Metallurgy and Materials, 57(2), 605–612. https://doi.org/10.2478/v10172-012-0064-x

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free