Abstract

We evaluated the activities of well-defined Ru@Pt core-shell nanocatalysts for hydrogen evolution and oxidation reactions (HER-HOR) using hanging strips of gas diffusion electrode (GDE) in solution cells. With gas transport limitation alleviated by micro-porous channels in the GDEs, the charge transfer resistances (CTRs) at the hydrogen reversible potential were conveniently determined from linear fit of ohmic-loss-corrected polarization curves. In 1 M HClO 4 at 23 °C, a CTR as low as 0.04 Ω cm -2 was obtained with only 20 μg cm -2 Pt and 11 μg cm -2 Ru using the carbon-supported Ru@Pt with 1:1 Ru:Pt atomic ratio. Derived from temperature-dependent CTRs, the activation barrier of the Ru@Pt catalyst for the HER-HOR in acids is 0.2 eV or 19 kJ mol -1. Using the Ru@Pt catalyst with total metal loadings <50 μg cm -2 for the HER in proton-exchange-membrane water electrolyzers, we recorded uncompromised activity and durability compared to the baseline established with 3 mg cm -2 Pt black.

Cite

CITATION STYLE

APA

Wang, J. X., Zhang, Y., Capuano, C. B., & Ayers, K. E. (2015). Ultralow charge-transfer resistance with ultralow Pt loading for hydrogen evolution and oxidation using Ru@Pt core-shell nanocatalysts. Scientific Reports, 5. https://doi.org/10.1038/srep12220

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free