Microstructure and Mechanical Behaviour of Ti-6Al-4V Matrix Reinforced with WCp Developed by Squeeze Casting

3Citations
Citations of this article
9Readers
Mendeley users who have this article in their library.

This article is free to access.

Abstract

The aim of this study is to evaluate the wear and micro hardness of a Ti-6Al-4V matrix reinforced with 10% and 15% tungsten carbide particle (WCp) composite manufactured using the squeeze casting process. Optical microscopy is used to determine the microstructures of the composite. A pin-on-disc wear test equipment and Vickers hardness at atmospheric temperature were used to examine the wear behaviour wear rate, CoF, and micro hardness qualities of primed samples. Loads of 10 N to 80 N, velocities of 4 m/s, and distances of 1000 m to 2000 m are considered for analyzing the wear behaviour of Ti-6Al-4V composites. The wear rate values are 25.683 for 10% WCp, 30.957 for 15% WCp, and 37.683 and 30.957 for 20% WCp. A scanning electron microscope (SEM) is utilized to examine the worn surface of the composites. For 10% WCp, the CoF values are 0.82 and 0.87, and for 15% WC, 0.88 and 0.956. The micro hardness values are 692 VHN for 10% WCp and 835 VHN for 15% WCp. The wear rate, microstructure, SEM images, coefficient of friction, and hardness of TMCs for totaling reinforcing tungsten carbide particle (WCp) possessions were discovered to be improved.

Cite

CITATION STYLE

APA

Sivakumar, R., Kumar, B. R. S., Subramaniyan, G. G., Sivaraja, M., Natarajan, M. P., Patil, P. P., … Abebe, K. J. (2022). Microstructure and Mechanical Behaviour of Ti-6Al-4V Matrix Reinforced with WCp Developed by Squeeze Casting. Journal of Nanomaterials, 2022. https://doi.org/10.1155/2022/6381265

Register to see more suggestions