Effect of thermocycling on the amount of monomer released from bulk fill composite resins

9Citations
Citations of this article
17Readers
Mendeley users who have this article in their library.

Abstract

The goal of this study was to examine the effect of thermal cycling on the amount of monomer released from bulk fill composites. Five bulk fill composite resins were used in the study. Extraction solutions were obtained at the end of the time/thermal cycle periods: 0–1 day/0–1,500, 1–3 days/1,500–4,500 and 3–7 days/4,500–10,000. The monomers in the extractions samples taken at each time point were measured on an HPLC instrument. The obtained data were analyzed by repeated measures of variance analysis and tukey multiple comparison tests (p<0.05). The thermocycling increased the amount of monomer released from all composites at 0–1 day (p<0.05). At 0–1 and 1–3 days, Venus Bulk Fill and Filtek Bulk Fill composite resins were more affected. Polymer networks with high molecular weight monomers such as Bis-GMA and UDMA can be less affected by thermal changes compared to polymers with low molecular weight monomers.

Cite

CITATION STYLE

APA

Hatipoǧlu, Ö., Karadaş, M., Er, H., & Turumtay, E. A. (2019). Effect of thermocycling on the amount of monomer released from bulk fill composite resins. Dental Materials Journal, 38(6), 1019–1025. https://doi.org/10.4012/dmj.2018-377

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free