In this work hot extrusion of hybrid composites of Al6061/SiC/Gr was carried out at ratios of 2:1,3:1&4:1 & temperatures of 4500,5000,&5500c at various compositions of 0,2,4,6 &8 % of SiC and fixed amount of graphite i.e 2% using 200 tonn capacity press at a speed of 1mm/sec to investigate mechanical properties like tensile, compression & BHN and after solutionising and aging. It was found that at ratio 3:1 and temperature 5000c all the above three properties were found to be improved compared to extrusion.

Cite

CITATION STYLE

APA

Balaji, M., Yerrennagoudar, H., & Veeresh Kumar, G. B. (2019). Effect of extrusion ratio & extrusion temperature on mechanical properties of hot extruded hybrid composites of al6061/sic/graphite. International Journal of Innovative Technology and Exploring Engineering, 8(11), 2821–2825. https://doi.org/10.35940/ijitee.K2316.0981119

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free