Fabrication of a Porous Low Refractive Index Anti-Reflective Coating with High Transmittance by Using the Porogen of Laureth-5 Carboxylic Acid

4Citations
Citations of this article
8Readers
Mendeley users who have this article in their library.

Abstract

A porous anti-reflective coating (P-ARC) with average transmittance in the visible range of 97.9% was fabricated through the sol-gel method, followed by calcination at a relatively low temperature (220 °C) using the porogen of Laureth-5 carboxylic acid via a one-step approach. The results demonstrated the coating had an absolute value that was 7.5% higher than that of bare glass (92%). The prepared porous anti-reflective coating had a refractive index as low as 1.21. The coating remained undamaged during 3M tape stripping tests while maintaining excellent light transmittance. This work presents a film that has good thermal stability, chemical stability, and mechanical stability.

Cite

CITATION STYLE

APA

Li, T., Tan, X., Chen, W., Zhang, F., Li, X., Liu, S., … Jiang, L. (2024). Fabrication of a Porous Low Refractive Index Anti-Reflective Coating with High Transmittance by Using the Porogen of Laureth-5 Carboxylic Acid. Coatings, 14(4). https://doi.org/10.3390/coatings14040440

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free