Water-related properties of pinus pinaster wood treated by different methods

4Citations
Citations of this article
9Readers
Mendeley users who have this article in their library.

Abstract

A study was made of water-related properties of Pinus pinaster wood impregnated with paraffin or modified by heat treatment or furfurylation. Treated woods were submerged in water for periods ranging from 2 to 1680 hours. Water absorption, swelling, and dimensional stability in the radial and tangential directions – expressed as Anti-Shrinking Efficiency (ASE) – were determined. Water absorption increased with time, reaching approximately 140% after 1680 h for untreated and heat-treated wood, and 60% for paraffinated and furfurylated wood. The rate of swelling differed between the first hours of soaking and after prolonged immersion. The final swelling was approximately 9% and 6% for untreated pine, 8% and 4% for paraffinated pine, 5.5% and 3% for heat-treated pine and 2.5% and 1% for furfurylated pine (in the tangential and radial directions respectively). At the end of the soaking test, furfurylated pine had the best ASE of approximately 80% and 70% in the tangential and radial directions respectively, followed by heat-treated pine with 44% and 34%, and paraffinated wood with 35% and 13%.

Cite

CITATION STYLE

APA

Domingos, I., Ferreira, J., Cruz-Lopes, L., & Esteves, B. (2018). Water-related properties of pinus pinaster wood treated by different methods. Drewno , 61(202), 69–80. https://doi.org/10.12841/wood.1644-3985.270.07

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free