Effect of different surface conditions on toughness of vanadis 6 cold work die steel-A review

4Citations
Citations of this article
15Readers
Mendeley users who have this article in their library.

Abstract

The effects of surface roughness, presence of nitrided diffusion regions, and magnetron sputtering of Cr2N-6Ag thin films on the toughness of Cr-V ledeburitic Vanadis 6 die steel were investigated by using the flexural strength measurement method, which was coupled with careful microstructural investigations and analyses of fractured surfaces. The results undoubtedly show that enhanced surface roughness reduces the material toughness, since the cusps formed on the metallic surface as a result of the machining act as preferential sites for crack nucleation and growth. The presence of nitrided regions on the surface, on the other hand, forms a structural notch there, which has a strong detrimental effect on toughness. Deposition of Cr2N-6Ag thin films has only marginal effect on the steel toughness. Practical recommendations for the designers, heat treaters, and coaters of the tools are thus that they should maintain the surface finish quality of the tools as high as possible, avoid too thick and supersaturated nitrided regions, and that there is almost no risk of tool embrittlement due to physical vapor deposition (PVD) coating.

Cite

CITATION STYLE

APA

Jurči, P. (2019, May 1). Effect of different surface conditions on toughness of vanadis 6 cold work die steel-A review. Materials. MDPI AG. https://doi.org/10.3390/ma12101660

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free