Failure prediction for Titanium alloys using a superplastic forming limit diagram approach

4Citations
Citations of this article
10Readers
Mendeley users who have this article in their library.
Get full text

Abstract

Superplastic forming limit diagrams (SPFLDs) are presented for both Ti-6A1-4V and Ti-6A1-2Sn-4Zr-2Mo alloys. FE-predieted ε1- ε3-ε̇eq paths for key points on the forming blank are then plotted on the SPFLD to predict failure, A key factor for reliable SPF forming limit prediction is the incorporation of a mechanisms-based constitutive model, which includes mierostruetural effects, such as static and dynamic grain growth and associated hardening, and with material constants independent of the forming strain-rate. The sinh model of Dunne and co-workers is thus employed. Results from forming trials for both materials are used to assess the failure predictions. © 2008 WILEY-VCH Verlag GmbH & Co. KGaA.

Cite

CITATION STYLE

APA

Leen, S. B., Kröhn, M. A., & Hyde, T. H. (2008). Failure prediction for Titanium alloys using a superplastic forming limit diagram approach. Materialwissenschaft Und Werkstofftechnik, 39(4–5), 327–331. https://doi.org/10.1002/mawe.200800299

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free