Adhesion between the resin shell and composite resin.

3Citations
Citations of this article
8Readers
Mendeley users who have this article in their library.

Abstract

Adhesiveness between the resin shell and composite resin was examined. As the resin shell, SR-PE-ISOCETTE, made from thermosetting crown and bridge resin, was used. The shear bond strengths between the resin shell and photocurable composite resin bonded by various methods were measured after 1-day of immersion in water at 37 degrees C. Super-bond C & B treatment to the resin shell effectively improved the adhesiveness, giving a bond strength of about 14 MPa. Clearfil new bond, Clearfil porcelain bond, Unifast and MMA/TBBO treatment gave almost the same bond strengths of about 7-9 MPa. Silane coupling agents were not effective for improving the bond strength. It was revealed that 4-META was necessary for obtaining good adhesion between SR-PE-ISOCETTE and composite resin.

Cite

CITATION STYLE

APA

Aida, M., Kanaya, H., Murata, Y., Hayakawa, T., & Horie, K. (1992). Adhesion between the resin shell and composite resin. The Journal of Nihon University School of Dentistry, 34(3), 167–171. https://doi.org/10.2334/josnusd1959.34.167

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free