Slow sintering in garnet-containing Y and Gd zirconate–aluminate mixtures for thermal barrier coatings

5Citations
Citations of this article
6Readers
Mendeley users who have this article in their library.

This article is free to access.

Abstract

Mixtures of rare-earth zirconates and aluminates containing Y or Y + Gd that form a two-phase garnet–fluorite mixture exhibit much slower sintering than pure fluorite at 1400°C. An equivalent Y-free, Gd-containing composition that forms a perovskite aluminate instead of garnet showed faster densification after the metastable garnet decomposes. At 1500°C, the Y-free sample also showed the fastest initial sintering rate, whereas there was more divergence in the sintering rate for the samples containing Y + Gd. The zirconate–aluminate with equimolar Y + Gd shows the slowest densification at 1500°C and retains ∼25% porosity after 250 h. The results highlight possibilities for designing compliant thermal barrier coatings that can retain significant porosity at 1400°C or higher.

Cite

CITATION STYLE

APA

Yu, Y. C., Godbole, E. P., Berrios, J., Hewage, N., & Poerschke, D. L. (2023). Slow sintering in garnet-containing Y and Gd zirconate–aluminate mixtures for thermal barrier coatings. Journal of the American Ceramic Society, 106(8), 4519–4525. https://doi.org/10.1111/jace.19121

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free