Abstract
The relative intensity ratios of the D band to the G band (ID/IG) used in Fig. 1b are incorrect in the original article. The value of ID/IG increases from 0.40 to 0.91 as the temperature is increased from 700 °C to 1000 °C. There are no errors in the original text. (Figure Presented). The Royal Society of Chemistry apologises for these errors and any consequent inconvenience to authors and readers.
Cite
CITATION STYLE
Correction: Zeolitic imidazolate framework (ZIF-8) derived nanoporous carbon: The effect of carbonization temperature on the supercapacitor performance in an aqueous electrolyte (Physical Chemistry Chemical Physics (2016) 8 (29308-29315) DOI: 10.1039/C6CP05555A). (2017). Physical Chemistry Chemical Physics. Royal Society of Chemistry. https://doi.org/10.1039/c7cp90179h