Optimization alkaline leaching of silicon element from bauxite ore

1Citations
Citations of this article
N/AReaders
Mendeley users who have this article in their library.

Abstract

The effect of alkaline leaching on the recovery of silicon elements from the Iraqi Bauxite Ore. was examined NaOH concentration, particle size, and stirring speed using the program MINITAB 16. NaOH concentration (X1) (1,2, and 4M), particle size (X2) (53,75, and 150µm), and stirring speed (X3) (250,500, and 750 rpm). The best recovery percentage was found to be (94.1097) when the variables were (X2= 53µM), (X1 = 4M), and (X3=750 rpm). The NaOH concentration (X1), particle size (X2), and stirring speed (X3) have a substantial influence on the process of recovery. However, NaOH concentration (X1) and particle size (X2) have a significant effect compared with the stirring speed (X3) on the recovery process.

Cite

CITATION STYLE

APA

Rashid, W. T. (2021). Optimization alkaline leaching of silicon element from bauxite ore. Al-Qadisiyah Journal for Engineering Sciences, 14(3), 173–178. https://doi.org/10.30772/qjes.v14i3.890

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free