Effect of roughness on perpendicular magnetic anisotropy in (Co90Fe10/Pt)n superlattices

21Citations
Citations of this article
23Readers
Mendeley users who have this article in their library.

This article is free to access.

Abstract

Superlattice [Co90Fe10(0.21)/Pt(0.23)]n (unit in nm) with the repeat cycles n ranging from 3 to 30 were studied. Both effective anisotropy (Keff) and PMA constant (KU) reached a maximum at n=8. When the 3 nm Pt underlayer was deposited at low energy condition, the Keff and KU of (CoFe/Pt)8 are 4.0 and 6.1 Merg/cc, respectively. On the other hand, the Keff and KU increased to 6.8 and 9.7 Merg/cc, respectively, when the Pt underlayer deposited at high energy condition. As the n increases, the surface roughness monotonously increases and d111 inside the superlattice layers increase and relax from bottom to top part. The interface roughness and relaxation in superlattice reduce the PMA considerably.

Cite

CITATION STYLE

APA

Qiu, J., Meng, Z., Yang, Y., Ying, J. F., Yap, Q. J., & Han, G. (2016). Effect of roughness on perpendicular magnetic anisotropy in (Co90Fe10/Pt)n superlattices. AIP Advances, 6(5). https://doi.org/10.1063/1.4944520

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free