Abstract

The geometrical factor in freckle formation has rarely been taken into account. In this work, freckle formation in superalloy components is examined. It is found that freckle formation is subject to the effects of the edge and curvature. In polygonal casting sections, freckles are formed preferably on the convex edges. In the components with a curved contour, freckles are exclusively formed on the outward-curving surface having positive curvature.

Cite

CITATION STYLE

APA

Ma, D. X., Dong, Z. H., Wang, F., & Dong, H. B. (2020). A Phenomenological Analysis of Freckling in Directional Solidification of Ni-Base Superalloy: The Role of Edge and Curvature in Casting Components. Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science, 51(1), 88–92. https://doi.org/10.1007/s11661-019-05513-5

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free