Abstract
Fresh water sponge was used as a silica source for the synthesis of MCM-41 via the hydrothermal process. The silica was extracted from the sponge by washing with nitric acid and piranha solution. Synthesis of MCM-41 was performed at 100 °C for 5 days and the procedure was optimized, with modifications made to the leaching temperature of the silica and the synthesis of mesoporous material, which was characterized by XRD, FT-IR, SEM and adsorption of N 2. The optimal result was achieved at a temperature of 135 °C for 3 days, showing ordered mesoporous material with a surface area of 1080 m 2 g-1.
Author supplied keywords
Cite
CITATION STYLE
Da Silva Lacerda, O., Cavalcanti, R. M., De Matos, T. M., De Brito Venâncio, J., De Barros, I. B., Da Veiga, V. F., & De Carvalho Lopes Barros, I. (2013). Síntese do material mesoporoso MCM-41 usando esponja de água-doce como fonte de sílica. Quimica Nova, 36(9), 1348–1353. https://doi.org/10.1590/S0100-40422013000900012
Register to see more suggestions
Mendeley helps you to discover research relevant for your work.