Abstract
PURPOSE. The purpose of this study is to evaluate the repair bond strength of a nanohybrid resin composite to three CAD/CAM blocks using different intraoral ceramic repair systems. MATERIALS AND METHODS. Three CAD/CAM blocks (Lava Ultimate, Cerasmart, and Vitablocks Mark II) were selected for the study. Thirty-two specimens were fabricated from each block. Specimens were randomly divided into eight groups for the following different intraoral repair systems: Group 1: control group (no treatment); Group 2: 34.5% phosphoric acid etching; Group 3: CoJet System; Group 4: Z-Prime Plus System; Group 5: GC Repair System; Group 6: Cimara System; Group 7: Porcelain Repair System; and Group 8: Clearfil Repair System. Then, nanohybrid resin composite (Tetric Evo Ceram) was packed onto treated blocks surfaces. The specimens were thermocycled before application of repair systems and after application of composite resin. After second thermal cycling, blocks were cut into bars (1 x 1 x 12 mm3) for microtensile bond strength tests. Data were analyzed using two-way ANOVA and Tukey's HSD test (α=.05). RESULTS. Cimara System, Porcelain Repair, and Clearfil Repair systems significantly increased the bond strength of nanohybrid resin composite to all CAD/CAM blocks when compared with the other tested repair systems (P
Author supplied keywords
Cite
CITATION STYLE
Gul, P., & Altinok-Uygun, L. (2020). Repair bond strength of resin composite to three aged CAD/CAM blocks using different repair systems. Journal of Advanced Prosthodontics, 12(3), 131–139. https://doi.org/10.4047/jap.2020.12.3.131
Register to see more suggestions
Mendeley helps you to discover research relevant for your work.