Magnetism and site occupancy in epitaxial Y-rich yttrium iron garnet films

23Citations
Citations of this article
23Readers
Mendeley users who have this article in their library.

Abstract

Y-rich yttrium iron garnet (Y-YIG) thin films were grown on gadolinium gallium garnet substrates using pulsed laser deposition from a YFeO3 target. The films are epitaxial on the substrate, and the unit cell of (001)- and (111)-oriented Y-YIG undergoes a tetragonal or rhombohedral distortion, respectively. The Y-YIG has lower room temperature magnetization but higher low-temperature magnetization than bulk YIG, and its Curie temperature was in the range of 330-400 K, depending on the growth conditions. First-principles calculations predict that YFe antisite defects are more stable in octahedral than tetrahedral Fe sites. Temperature-dependent magnetization measurements together with a superexchange dilution model and composition determined from x-ray photoelectron spectroscopy indicate that nonmagnetic species (Y3+ and vacancies) are predominantly accommodated in the octahedral sites, but there is a significant occupancy of tetrahedral sites.

Cite

CITATION STYLE

APA

Su, T., Ning, S., Cho, E., & Ross, C. A. (2021). Magnetism and site occupancy in epitaxial Y-rich yttrium iron garnet films. Physical Review Materials, 5(9). https://doi.org/10.1103/PhysRevMaterials.5.094403

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free