PERBANDINGAN UJI KEBOCORAN TEPI RESIN KOMPOSIT FLOWABLE DAN BAHAN LUTING SEMEN PADA PASAK POLYETHYLENE FIBER-REINFORCED (PFR)

  • Nasrudin M
  • Aju Fatmawati D
  • Soesetijo F
N/ACitations
Citations of this article
38Readers
Mendeley users who have this article in their library.

Abstract

Background: Zinc phosphate, glass-ionomer, and resin cement are the most commonly used as luting cements. Flowable composite resin could reduce restoration microleakage and provided better marginal seal in dentin. Purpose: The objective of the study was to compare microleakage between flowable composite resin and cement luting materials.Methods: The study was experimental laboratory by the post test only without control group design. The sample size was 18, which was divided into 3 groups. Each group consisted of 6 samples. Glass-ionomer cement and zinc phosphate were luting cement materials that used in the study. Microleakage measurement method used stereomicroscope after the samples were stored in methylen blue 0.25%.Results: The smallest average value of microleakage was in the flowable composite resin group (29,16%). One way ANOVA test results showed that there were significant differences between treatment groups (p=0.000). Conclusion: It was concluded that flowable composite resin have smaller microleakage average value than glass-ionomer cement and zinc phosphate.

Cite

CITATION STYLE

APA

Nasrudin, M., Aju Fatmawati, D. W., & Soesetijo, F. A. (2016). PERBANDINGAN UJI KEBOCORAN TEPI RESIN KOMPOSIT FLOWABLE DAN BAHAN LUTING SEMEN PADA PASAK POLYETHYLENE FIBER-REINFORCED (PFR). ODONTO : Dental Journal, 3(1), 27. https://doi.org/10.30659/odj.3.1.27-33

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free