Viscoelastic stress/strain behavior of pharmaceutical tablets: Analysis during unloading and postcompression periods

97Citations
Citations of this article
42Readers
Mendeley users who have this article in their library.
Get full text

Abstract

The processes of nonequilibrium generation and decay of axial and radial stresses within tablet compacts were analyzed in terms of three‐dimensional linear viscoelastic theory. A rotary tablet press was instrumented to measure punch and die wall stresses during the compression and postcompression periods. Following compression, tablets were permitted to remain at the compression site within the die, and the die wall stress was followed. Microcrystalline cellulose, spray‐processed lactose, and sulfacetamide are known to have different compression characteristics and were found to differ significantly in their viscoelastic parameters. Compacts assumed their final viscoelastic state prior to the time of punch separation. Theory permits separation of material behavior into dilation and distortion components. Dilation, thought to be dependent on voids, was elastic in all cases. Distortion effects could be described well by a Kelvin solid model. Results indicate that viscoelastic properties are functions of compression conditions and may be useful in adjusting compression conditions to avoid problems such as capping. Copyright © 1981 Wiley‐Liss, Inc., A Wiley Company

Cite

CITATION STYLE

APA

Rippie, E. G., & Danielson, D. W. (1981). Viscoelastic stress/strain behavior of pharmaceutical tablets: Analysis during unloading and postcompression periods. Journal of Pharmaceutical Sciences, 70(5), 476–482. https://doi.org/10.1002/jps.2600700503

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free