Abstract
The hydrogenation of Nd 2 Fe 14 B under a high pressure of hydrogen has been investigated for the first time. At the heat-treatment temperature of 600°C, almost complete decomposition of Nd 2 Fe 14 B into NdH 2+x and α-Fe is observed, although a rather long heat-treatment time is necessary to achieve the sufficient hydrogenation. The desorption of hydrogen from NdH 2+x does not occur in the furnace-cooling process.
Author supplied keywords
Cite
CITATION STYLE
Kataoka, Y., Kawamoto, Y., Ono, T., Tsubota, M., & Kitagawa, J. (2015). Hydrogenation of Nd-Fe-B magnet powder under a high pressure of hydrogen. Results in Physics, 5, 99–100. https://doi.org/10.1016/j.rinp.2015.04.001