Abstract
The precipitation of the γ′, γ″ and δ phases in a spray-formed version of IN 718 has been studied by hardness measurement and metallographic examination of samples subjected to solution treatment at 1025°C followed by isothermal treatments between 620 and 1010°C up to 100 h. The precipitation processes were compared to those in a wrought (ring-rolled) version of the alloy subjected to the same heat treatments. Time-temperature-hardness diagrams for the two alloys were constructed. Small differences were observed between the two materials but these can at least partly be attributed to differences in composition. For the spray-cast material the δ-phase solvus temperature was determined and the growth kinetics of the γ″ phase established.
Cite
CITATION STYLE
Azadian, S., Wei, L. Y., Niklasson, F., & Warren, R. (2001). Precipitation in spray-formed in 718. In Proceedings of the International Symposium on Superalloys and Various Derivatives (Vol. 1, pp. 617–626). Minerals, Metals and Materials Society. https://doi.org/10.7449/2001/superalloys_2001_617_626
Register to see more suggestions
Mendeley helps you to discover research relevant for your work.