Stopping power of fluorides and semiconductor organic films for low-velocity protons

21Citations
Citations of this article
19Readers
Mendeley users who have this article in their library.

Abstract

A combined experimental and theoretical study of the energy loss of protons in fluorides and organic films is presented. The measurements were performed in fresh AlF3, LiF, and N,N′-bis(1-ethylpropyl)-perylene-3,4,9,10- tetracarboxdiimide (EP-PTCDI) evaporated in situ on self-supported C or Ag foils, covering the very low energy range from 25 keV down to 0.7 keV. The transmission method is used in combination with time-of-flight (TOF) spectrometry. In the case of fluorides with large band gap energies (AlF3 and LiF), the experimental stopping power increases almost linearly with the mean projectile velocity showing a velocity threshold at about 0.1 a.u. These features are well reproduced by a model based on quantum scattering theory that takes into account the velocity distribution and the excitation of the active 2p electrons in the F- anions, and the properties of the electronic bands of the insulators. In the case of the semiconductor organic film with a lower gap, the experimental stopping power increases linearly with the mean projectile velocity without presenting a clear threshold. This trend is also reproduced by the proposed model. © 2010 The American Physical Society.

Cite

CITATION STYLE

APA

Serkovic Loli, L. N., Sánchez, E. A., Grizzi, O., & Arista, N. R. (2010). Stopping power of fluorides and semiconductor organic films for low-velocity protons. Physical Review A - Atomic, Molecular, and Optical Physics, 81(2). https://doi.org/10.1103/PhysRevA.81.022902

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free